Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® B3ZG8 BK20560 - PA6-I-GF40 - BASF

Material Data Center offers the following functions for Ultramid® B3ZG8 BK20560:
unit conversion, PDF datasheet print, comparison with other plastics, application examples, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultramid B datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Impact-modified, glass fiber reinforced injection molding grade for industrial items having very high impact strength and rigidity, used e.g. for automobile airbag housings and half-shells for suitcases.
Caratteristiche Fisichesecco/condUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 10 / * cm³/10min ISO 1133
Temperatura 275 / * °C -
Carico 5 / * kg -
Ritiro di stampaggio, parallelo 0.3 / * % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 0.7 / * % ISO 294-4, 2577
Proprietà Meccanichesecco/condUnitáNorma del test
ISO Data
Modulo a trazione 11600 / 6700 MPa ISO 527
Carico unitario a rottura 160 / 115 MPa ISO 527
Deformazione a rottura 4.9 / 9.5 % ISO 527
Resistenza all'urto Charpy, +23°C 110 / 130 kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C 105 / 110 kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 24 / 40 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, -30°C 15 / 13.7 kJ/m² ISO 179/1eA
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 220 / * °C ISO 11357-1/-3
Temp.di inflessione sotto carico, 1.80 MPa 205 / * °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 220 / * °C ISO 75-1/-2
Coeff.di dilatazione termica lin., parallelo 18 / * E-6/K ISO 11359-1/-2
Coeff.di dilatazione termica lin., perpend. 125 / * E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm HB / * class IEC 60695-11-10
Spessore provato 1.6 / * mm -
Yellow Card disponibile sì / * - -
Reazione al fuoco a spessore h HB / * class IEC 60695-11-10
Spessore provato 0.7 / * mm -
Yellow Card disponibile sì / * - -
Indice di ossigeno 23 / * % ISO 4589-1/-2
Proprietà Elettrichesecco/condUnitáNorma del test
ISO Data
Costante dielettrica relativa, 1MHz 4 / 5.3 - IEC 62631-2-1
Fattore di dissipazione, 1MHz 200 / 1300 E-4 IEC 62631-2-1
Resistività volumica 1E13 / 1E10 Ohm*m IEC 62631-3-1
Resistività superficiale * / 1E10 Ohm IEC 62631-3-2
Res. Alle correnti striscianti superficiali - / 550 - IEC 60112
Altre Proprietàsecco/condUnitáNorma del test
Assorbimento d'acqua 5 / * % Sim. alla ISO 62
Assorbimento d'umidità 1.6 / * % Sim. alla ISO 62
Massa volumica 1400 / - kg/m³ ISO 1183
Proprietà Specifiche Materialesecco/condUnitáNorma del test
ISO Data
Numero di viscosità 160 / * cm³/g ISO 307, 1157, 1628
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 80 °C -
Pre-essiccamento - Tempo 4 h -
Umidità del Processo ≤0.15 % -
Temperatura di fusione 270 - 290 °C -
Temperatura dello stampo 80 - 90 °C -
Funzioni
Viscosità-Velocità di taglio , Ultramid® B3ZG8 BK20560, PA6-I-GF40, BASF
Sforzo di taglio-Velocità di taglio , Ultramid® B3ZG8 BK20560, PA6-I-GF40, BASF
Sforzi-deformazione , Ultramid® B3ZG8 BK20560 (Secco), PA6-I-GF40, BASF
Sforzi-deformazione , Ultramid® B3ZG8 BK20560 (cond.), PA6-I-GF40, BASF
Modulo secante-deformazione , Ultramid® B3ZG8 BK20560 (Secco), PA6-I-GF40, BASF
Modulo secante-deformazione , Ultramid® B3ZG8 BK20560 (cond.), PA6-I-GF40, BASF
Sforzi-deformazioni (isocrona) 23°C, Ultramid® B3ZG8 BK20560 (cond.), PA6-I-GF40, BASF
Modulo di scorrimento-tempo 23°C, Ultramid® B3ZG8 BK20560 (cond.), PA6-I-GF40, BASF
Curva di scorrimento 23°C, Ultramid® B3ZG8 BK20560 (cond.), PA6-I-GF40, BASF
Sforzi-deformazioni (isocrona) 90°C, Ultramid® B3ZG8 BK20560 (Secco), PA6-I-GF40, BASF
Modulo di scorrimento-tempo 90°C, Ultramid® B3ZG8 BK20560 (Secco), PA6-I-GF40, BASF
Curva di scorrimento 90°C, Ultramid® B3ZG8 BK20560 (Secco), PA6-I-GF40, BASF
Sforzi-deformazioni (isocrona) 120°C, Ultramid® B3ZG8 BK20560 (Secco), PA6-I-GF40, BASF
Modulo di scorrimento-tempo 120°C, Ultramid® B3ZG8 BK20560 (Secco), PA6-I-GF40, BASF
Curva di scorrimento 120°C, Ultramid® B3ZG8 BK20560 (Secco), PA6-I-GF40, BASF
Sforzi-deformazioni (isocrona) 160°C, Ultramid® B3ZG8 BK20560 (Secco), PA6-I-GF40, BASF
Modulo di scorrimento-tempo 160°C, Ultramid® B3ZG8 BK20560 (Secco), PA6-I-GF40, BASF
Curva di scorrimento 160°C, Ultramid® B3ZG8 BK20560 (Secco), PA6-I-GF40, BASF
Volume specifico-temperatura (pvT) , Ultramid® B3ZG8 BK20560, PA6-I-GF40, BASF
Modulo a taglio-temperatura , Ultramid® B3ZG8 BK20560 (Secco), PA6-I-GF40, BASF
Modulo a taglio-temperatura , Ultramid® B3ZG8 BK20560 (cond.), PA6-I-GF40, BASF
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Forma fisica disponibile
Pellet, Nero
Additivi
Lubrificanti, Agente di distacco
Caratteristiche speciali
Alto urto o modificato all'urto, Stabilizzato o stabile al calore
Applicazioni
Automotive
Disponibilità geografica
Altre informazioni
Stampaggio ad Iniezione
PREPROCESSING
Pre/Post-processing, max. allowed water content: .15 %
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 270 - 290 °C
injection molding, Melt temperature, recommended: 280 °C
injection molding, Mold temperature, range: 80 - 90 °C
injection molding, Mold temperature, recommended: 80 °C
injection molding, Dwell time, thermoplastics: 10 min
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.